Report of Committee on Concrete Roads and Pavements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Report of Committee on Concrete Roads and Pavements

Author(s): ACI Committee on Concrete Roads and Pavements

Publication: Journal Proceedings

Volume: 17

Issue: 2

Appears on pages(s): 297-298

Keywords: none

DOI: 10.14359/15720

Date: 2/1/1921

Abstract:
Your Committee on Concrete Roads and Pavements realizes that the world has progressed and our knowledge of concrete road construction has increased in some particulars since the Recommended Practice of the Institute was adopted. However, your committee is of the opinion that advances commonly accepted along this line have not been radical.