Title: Standard Concrete Highway Bridges and Culverts

Author(s): A.C. Irwin

Publication: Journal Proceedings

Volume: 17

Issue: 2

Appears on pages(s): 90-110

Keywords: none

DOI: 10.14359/15707

Date: 2/1/1921

Abstract:
Concrete is now serving as the material of which highway bridges are constructed for all sorts of openings, ranging from a small diameter single concrete pipe culvert to the enormous arch span of 400 ft. now under construction over the Mississippi River at Minneapolis, Minn.