Title: Concrete Products Plant Operation

Author(s): ACI Committee P-6

Publication: Journal Proceedings

Volume: 18

Issue: 2

Appears on pages(s): 260-276

Keywords: none

DOI: 10.14359/15694

Date: 2/1/1922

Abstract:
From year to year as the activities of the American Concrete Istitute expand, they come more and more in contact with a concrete industry that has been struggling aslong practically unaided by scientific research. Every step of progess has been contested by strongly combined competitors. Regardless of all this opposition, that industry, the concrete products industry, has interested thousands of investors who have put over fifty millions of dollars into factories making various kinds of products.