Reinforced-Concrete Chimneys

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reinforced-Concrete Chimneys

Author(s): ACI Committee S-1

Publication: Journal Proceedings

Volume: 18

Issue: 2

Appears on pages(s): 221-224

Keywords: none

DOI: 10.14359/15688

Date: 2/1/1922

Abstract:
The committee has prepared the substance of a specification for the design and construction of tapering reinforced-concrete chimneys. The intent of these specifications is to provide for the design and construction of tapering reinforced-concrete chimneys and their foundations.