Monolithic Concrete House Construction at Phillipsburg, N.J.

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Monolithic Concrete House Construction at Phillipsburg, N.J.

Author(s): Paul R. Smith

Publication: Journal Proceedings

Volume: 18

Issue: 2

Appears on pages(s): 141-150

Keywords: none

DOI: 10.14359/15678

Date: 2/1/1922

Abstract:
In 1918, when the Ingersoll Rand Co., of Phillipsburg, N.J., wished to construct houses for employees, little thought had been give as to the kind of house which would be erected. It was necessary, first to build houses rapidly, economically, to make them attractive and comfortable and suit the needs of of the various classes of people for whom the houses were intended.