Gun-Stone House at Watertown, Massachusetts

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Gun-Stone House at Watertown, Massachusetts

Author(s): H. Whittemore Brown

Publication: Journal Proceedings

Volume: 18

Issue: 2

Appears on pages(s): 131-139

Keywords: none

DOI: 10.14359/15677

Date: 2/1/1922

Abstract:
A concrete house has recently been constructed in Watertown, Mass., that is the result of considerable research on the problem of constructing a house which would combine as many of the following principles as possible: 1. Maximum protection form the elements. 2. Economical use of materials. 3. Indestructible by fire or elements. 4. Attractive interior surfaces. The result of this research is the system of construction which has been termed "Gun-Stone," because of the combination of gunite and concrete.