A Special Type of Floor Finish

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Special Type of Floor Finish

Author(s): W. M. Bailey

Publication: Journal Proceedings

Volume: 18

Issue: 2

Appears on pages(s): 122-123

Keywords: none

DOI: 10.14359/15675

Date: 2/1/1922

Abstract:
Before laying the type of floor finish described in this paper, a number of tests were made on various kinds of concrete surfaces to determine the one having the greatest resistance to wear and best adapted to the severe wearing conditions and occuring in industrial plants. The problem was considered with reference to (a) materials incorporated in the finish and (b) method of laying the finish.