Flexural Strength of Plain Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural Strength of Plain Concrete

Author(s): Duff A. Abrams

Publication: Journal Proceedings

Volume: 18

Issue: 2

Appears on pages(s): 20-45

Keywords:

DOI: 10.14359/15670

Date: 2/1/1922

Abstract:
The flexural strength of concrete is low as compared with its compressive stregth; the use of steel bars to supply this deficiency is the basic prinicple of reinforced concrete construction.