Joint Concrete Culvert Pipe Committee

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Joint Concrete Culvert Pipe Committee

Author(s): ACI Committee J-2

Publication: Journal Proceedings

Volume: 19

Issue: 1

Appears on pages(s): 292-293

Keywords: none

DOI: 10.14359/15650

Date: 1/1/1923

Abstract:
The tests referred to in the previous report have been continued and much valuable data secured. The object of these test was to secure information covering loads on culverts in railroad and highway embankments and if possible to discover the laws of variation of such loads. Although these tests are not yet concluded we have in general found certain underlying prinicples to be involved. The ability of a culvert pipe to carry a load after it has been built into a culvet depends on construction conditions as well as upon the strength of the pipe itself.