Title: Quality Control in Concrete Products Plants

Author(s): Stanton Walker

Publication: Journal Proceedings

Volume: 19

Issue: 1

Appears on pages(s): 88-99

Keywords: none

DOI: 10.14359/15635

Date: 1/1/1923

Abstract:
The present day concrete products manufacturer shows a marked interest in the quality of his product and means for controlling it. This is evidenced by the progressive spirit shown by local and national organizations of manufactures . . . The object of this paper is to point out the fundamental principles involved in concrte mixtures and their application to the work of the concrete products manufacturer. The principles described were developed at the Structural Materials Research Laboratory. The reasearch work of this laboratory is being carried out through the cooperation of Lewis Institute and the Portland Cement Association, under the direction of Prof. Duff A. Abrams.