Design of Elastic Structures from Paper Models

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design of Elastic Structures from Paper Models

Author(s): George Erle Beggs

Publication: Journal Proceedings

Volume: 19

Issue: 1

Appears on pages(s): 53-65

Keywords: none

DOI: 10.14359/15632

Date: 1/1/1923

Abstract:
This paper is supplementary to the one on a similar subject given before this Society a year ago. My purpose here is first, to present additional evidence of the correctness of the results obtained from the deflections of paper models; and, second, to indicate some of the practical uses of the model method of analysis.