A New Method of Constructing Reinforced-Concrete Water Tanks

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A New Method of Constructing Reinforced-Concrete Water Tanks

Author(s): W.S. Hewett

Publication: Journal Proceedings

Volume: 19

Issue: 1

Appears on pages(s): 41-52

Keywords: none

DOI: 10.14359/15631

Date: 1/1/1923

Abstract: