Title: Joint Concrete Culvert Pipe Committee

Author(s): ACI Committee J-2

Publication: Journal Proceedings

Volume: 25

Issue: 2

Appears on pages(s): 606-621

Keywords: none

DOI: 10.14359/15591

Date: 2/1/1929

Abstract:
The Joint Concrete Culvert Pipe Committee was organized in 1919 to prepare standard specifications for reinforced concrete pipe to be used for railway and highway culverts. The committee has held one or more meetings each year since its organization and in February, 1926, it presented to the constituent organizations a report embodying recommended tentative standard specifications for reinforced concrete culvert pipe. That report was very widely distributed; more than 5,000 copies being furnished to public officials and manufacturers and users of pipe in the United States and Canada.