Standard Building Units

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Standard Building Units

Author(s): ACI Committee P-1

Publication: Journal Proceedings

Volume: 25

Issue: 2

Appears on pages(s): 602-604

Keywords: none

DOI: 10.14359/15590

Date: 2/1/1929

Abstract:
Your committee on Standard Concrete Building Units cooperated with the American Society for Testing Materials and the Federal Specifications Board in an effort to obtain uniform requirements in specifications for concrete brick.