Title: Report of Tests on Concrete Building Tile

Author(s): ACI Committee P-1

Publication: Journal Proceedings

Volume: 23

Issue: 2

Appears on pages(s): 691-693

Keywords: none

DOI: 10.14359/15574

Date: 2/1/1927

Abstract:
The purpose of these tests was to study the effect of various gradings of aggregate having the same fineness moduli on the strength and absorption of tamped concrete building tile. The tests were made under the auspices of Committee P-1, American Concrete Institute. Acknowledgment is made to Prof. R. L. Morrison who tested the tile and the cement at the Michigan State Highway Laboratory, Ann Arbor, and to E. W. Dienhart, who furnished materials and the plant of Acme Concrete Products and Gravel Co., Cement City, Mich., where the specimens were made by C.L. Bourne, representing the committee.