Title:
Concrete Products Plant Operation
Author(s):
ACI Committee P-6
Publication:
Journal Proceedings
Volume:
22
Issue:
2
Appears on pages(s):
673
Keywords:
none
DOI:
10.14359/15562
Date:
2/1/1926
Abstract:
Committee P-6 felt that it would be desirable to elaborate on the curing tests reported at the 1925 convention to cover curing conditions during the whole year. A sub-committee on curing was appointed which outlined a series of tests to determine the effect of weather conditions on the outdoor curing of concrete block.