Title: Standard Specifications for Concrete Brick

Author(s): ACI Committee P-1

Publication: Journal Proceedings

Volume: 21

Issue: 2

Appears on pages(s): 604-605

Keywords: none

DOI: 10.14359/15552

Date: 2/1/1925

Abstract:
The purpose of these specifications is to define the requirements for concrete brick to be used in construction.