Tentative Standard Specfication on Measurement of and Estimating Concrete-Standard Methods for the Measurement of Concrete Work

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tentative Standard Specfication on Measurement of and Estimating Concrete-Standard Methods for the Measurement of Concrete Work

Author(s): ACI Committee C-5

Publication: Journal Proceedings

Volume: 21

Issue: 2

Appears on pages(s): 576-582

Keywords: none

DOI: 10.14359/15546

Date: 2/1/1925

Abstract:
The following divisions are recognized as separate and distinct operations in the construction of concrete work for which separate modes of measurement are necessary.