Standard Specifications for Portland Cement Concrete Pavements: Two-Course Portland Cement Concrete Pavement for Highways

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Standard Specifications for Portland Cement Concrete Pavements: Two-Course Portland Cement Concrete Pavement for Highways

Author(s): ACI Committee S-6

Publication: Journal Proceedings

Volume: 20

Issue: 2

Appears on pages(s): 710-715

Keywords: none

DOI: 10.14359/15525

Date: 2/1/1924

Abstract:
It is the intent of these specifications to cover the requirements for materials and construction of Portland Cement Concrete Pavement composed of two layers of concrete made with unlike coarse aggregates, but of the same proportions.