Expansion Joints in Concrete Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Expansion Joints in Concrete Construction

Author(s): ACI Committee E-8

Publication: Journal Proceedings

Volume: 20

Issue: 2

Appears on pages(s): 619-632

Keywords: none

DOI: 10.14359/15513

Date: 2/1/1924

Abstract:
The Committee on Expansion Joints in Concrete Construction submits, for the purpose of discussion, the following summary of the problem of expansion joints, with a certain amount of information concerning the materials usually employed in such work. Typical sections are shown of expansion joints of different types.