The Relation Between the Wall Thickness and Diameter of Concrete Culvert Pipe for Highway Use

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Relation Between the Wall Thickness and Diameter of Concrete Culvert Pipe for Highway Use

Author(s): G.W. Hutchinson

Publication: Journal Proceedings

Volume: 20

Issue: 2

Appears on pages(s): 237-246

Keywords: none

DOI: 10.14359/15497

Date: 2/1/1924

Abstract:
The manufacture of concrete culvert pipe appears to be an easy task. On the contrary, it is a matter which requires considerable study if an economic product is to be secured and also is one in which continual improvement is possible.