The Earthquake in Japan

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Earthquake in Japan

Author(s): Joseph S. Ruble

Publication: Journal Proceedings

Volume: 20

Issue: 2

Appears on pages(s): 210-220

Keywords: none

DOI: 10.14359/15495

Date: 2/1/1924

Abstract:
The first earthquake shock on September 1, 1923, was at 11.50 a. m., the second about ¾ of a min. later, the third about 3 ½ min. later, and the fourth 11 min. later. The maximum intensity of the shock resulted in a horizontal motion, as recorded at the Imperial University in Tokyo, of 5 ½ in.