Fire Resistance of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fire Resistance of Concrete

Author(s): ACI Committee E-4

Publication: Journal Proceedings

Volume: 21

Issue: 2

Appears on pages(s): 284-299

Keywords: none

DOI: 10.14359/15482

Date: 2/1/1925

Abstract:
Committee E-4 on Fire Resistance of Concrete was authorized by the Board of Direction at a meeting held in April, 1923. The purpose of the committee was the “study and review of test data and the make a report as early as possible on the comparative fire resistance of these various types of concretes with special reference to the kind of aggregate."