Inundation as a Practical Aid to Uniform Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Inundation as a Practical Aid to Uniform Concrete

Author(s): Arthur A. Levison

Publication: Journal Proceedings

Volume: 21

Issue: 2

Appears on pages(s): 216-225

Keywords: none

DOI: 10.14359/15478

Date: 2/1/1925

Abstract:
The last few years have brought a keen realization that concrete as made for construction purposes is notably lacking in uniformity of quality.