Abstract:
The establishment of central plants for the production of ready-mixed concrete was suggested by the successful operation of similar plants for concrete highway paving. Mixed concrete from such plants is frequently hauled four or fice miles with satisfactory results. With this in mind it is natural that progressive material dealers should recognize the possibilities for the sale of ready-mixed concrete, as well as the sale of the new materials.