Crazing on Cement Products

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Crazing on Cement Products

Author(s): P.H. Bates

Publication: Journal Proceedings

Volume: 21

Issue: 2

Appears on pages(s): 126-130

Keywords: none

DOI: 10.14359/15470

Date: 2/1/1925

Abstract:
The title is purposely chosen because the three common products using cement, as a bond all show crazing. This difficulty is not restricted either to neat cement or mortar or concrete. So far as cement products are concerned we are all familiar with the manifestation of crazing. Some believe they know the cause of this and a, still smaller number believe they know how to prevent it. (Parenthetically, they are eligible for membership on this committee provided they will demonstrate facts and not present theories.) Consequently this paper will not discuss crazing objectively but metaphorically and subjectively.