Title: The Effect of Varied Curing Conditions Upon the Compressive Strength of Mortars and Concretes

Author(s): Herbert J. Gilkey

Publication: Journal Proceedings

Volume: 22

Issue: 2

Appears on pages(s): 395-431

Keywords: none

DOI: 10.14359/15455

Date: 2/1/1926

Abstract:
The curing conditions considered are only those dependent upon the effect of moisture, or the lack of it, on the strength of portland cement mortars and concretes. Other important factors, such as temperature changes, impure curing waters, etc., are not here considered.