Title: New Experiences in Concrete Control

Author(s): John G. Ahlers

Publication: Journal Proceedings

Volume: 22

Issue: 2

Appears on pages(s): 159-195

Keywords: none

DOI: 10.14359/15441

Date: 2/1/1926

Abstract:
There is accumlating a large collection of literature on the subject of design of concrete and its simple presentation or method of control. This paper is written in an attempt to clarify the problem so that in the end good uniform concrete of even strength will be obtained by simple methods and hence much less detail of supervision.