Use of the Water-Ratio Specification on the Portland Cement Association Building

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of the Water-Ratio Specification on the Portland Cement Association Building

Author(s): F.R. McMillan and Stanton Walker

Publication: Journal Proceedings

Volume: 22

Issue: 2

Appears on pages(s): 122-156

Keywords: none

DOI: 10.14359/15440

Date: 2/1/1926

Abstract:
The quality of concrete in the office and laboratory building of the Portland Cement Association was successfully controlled, without the use of special equipment and without the need of a testing organization, solely by means of a specification based on the control of the quantity of mixing water. This specification fixed only the proportion of water to cement; the aggregate proportions were left entirely to the judgement of the contractor, with the limitation that plastic and workable mixes be produced.