Title: Time as a Factor in Making Concrete-Centrifugal Pipe Manufacture

Author(s): F.F. Longley

Publication: Journal Proceedings

Volume: 23

Issue: 2

Appears on pages(s): 481-482

Keywords: none

DOI: 10.14359/15430

Date: 2/1/1927

Abstract:
In the manufacture of centrifugal pipe, the manipulation of the concrete immediately after mixing, is done in a way that results in a very low water ratio at the time effective hydration of the cement and setting of the concrete commences.