What Workability Means to the Contractor

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: What Workability Means to the Contractor

Author(s): Nelson L. Doe

Publication: Journal Proceedings

Volume: 24

Issue: 2

Appears on pages(s): 77-82

Keywords: none

DOI: 10.14359/15377

Date: 2/1/1928

Abstract:
During the past five years remarkable progress in the making and placing of concrete has been made. The contractor of today realizes that a properly designed mix which will produce workable concrete is necessary. Furthermore, the up-to-date contractor is well aware that workable concrete is much more economical, as to cost of materials and expense of handling than the average concrete made without a calculated mix.