Purchasing Centrally Mixed Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Purchasing Centrally Mixed Concrete

Author(s): P.J. Freeman

Publication: Journal Proceedings

Volume: 25

Issue: 2

Appears on pages(s): 632-635

Keywords: none

DOI: 10.14359/15357

Date: 2/1/1929

Abstract:
The development of central mixing plants during the past few years has necessitated a revision of specifications as well as of general ideas concerning mixing and handling concrete. In 1925 there were about 25 such plants and today there are at least 100 concerns making and selling ready-mixed concrete.