The Physical Properties of Commercial Cast Stone

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Physical Properties of Commercial Cast Stone

Author(s): John Tucker, Jr. and G.W. Walker

Publication: Journal Proceedings

Volume: 25

Issue: 2

Appears on pages(s): 501-513

Keywords: none

DOI: 10.14359/15352

Date: 2/1/1929

Abstract:
As a result of a desire on the part of the Federal departments for a specification for cast stone, the Bureau of Standards has undertaken at the request of the Federal Specifications Board, the accumulation of data on the physical properties of commercial cast stone upon which such a specification may be written. Existing published data upon the properties of cast stone being very meager, the manufacturers and builders with whom the Bureau has been in contact are also keenly interested in having these properties determined. This paper presents some of the data which have been accumulated to date during this study and is in the nature of a progress report of an investigation in which much more remains to be done.