Concrete Studies at the Bull Run Dam, City of Portland, Oregon

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Studies at the Bull Run Dam, City of Portland, Oregon

Author(s): T.C. Powers

Publication: Journal Proceedings

Volume: 25

Issue: 2

Appears on pages(s): 388-420

Keywords: none

DOI: 10.14359/15350

Date: 2/1/1929

Abstract:
The problem of estimating the strength of concrete containing aggregate too large for the test specimen is studied. In addition to the water-cement ratio, two more variables are introduced, (1) the paste content (paste is cement plus water) and, (2) the physical condition of the paste at the time of hardening, i.e., its homogeneity. The latter variable is shown to influence permeability as well as strength. The dependence of the water-cement-ratio-strength relation upon the other two variables is discussed, and conditions are cited under which it does not exist at all. The modulus of elasticity appears to be greatly influenced by the paste content.