Concrete—the Sustainable Construction Material

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete—the Sustainable Construction Material

Author(s): Mette Glavind, Jacob Mehus, Gisli Gudmundsson, Per Fidjestol

Publication: Concrete International

Volume: 28

Issue: 5

Appears on pages(s): 41-44

Keywords: aggregate; supplementary cementitious materials; sustainability; thermal mass

DOI:

Date: 5/1/2006

Abstract:
In 2003, members of the Nordic concrete industry gathered for an international conference to present the status of research and development activities related to environmental issues. Among the topics discussed were supplementary cementitious materials, creative applications of concrete for environmental protection, and alternative aggregates. The Nordic consensus definitions of sustainable development and environmentally sustainable concrete structures and an overview of the conference and subsequent activities are provided in this article.