Title: LEED Rating and Tilt-up

Author(s): Kimberly Waggle Kramer

Publication: Concrete International

Volume: 28

Issue: 5

Appears on pages(s): 32-34

Keywords: LEED; sustainability; tilt-up concrete; wall panels

DOI:

Date: 5/1/2006

Abstract:
To meet LEED requirements, practitioners must design and specify systems with attributes listed as desirable by the USGBC. Tilt-up concrete walls can help contribute LEED points in several categories through their durability, ease of recycling, ability to help moderate temperature swings, recycled materials content, and use of local materials. A brief introduction to these categories is provided in this article.