Flexural Behavior of Reinforced Masonry Panels

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural Behavior of Reinforced Masonry Panels

Author(s): Joaquim A. O. Barros, Juliana T. Oliveira, Everaldo Bonaldo, and Paulo B. Lourenco

Publication: Structural Journal

Volume: 103

Issue: 3

Appears on pages(s): 418-426

Keywords: clay; joint; masonry; stiffening

DOI: 10.14359/15320

Date: 5/1/2006

Abstract:
A new industrialized solution for construction of reinforced brick masonry shell roofs was recently developed. Here, the influence of both the brick and reinforcement arrangements on the flexural behavior of this structural system is analyzed by carrying out four-point bending tests with reinforced masonry panels. The panel structural system is made from clay bricks, reinforced concrete joints, and a concrete layer reinforced with welded wire mesh. The panel positive flexural resistance (concrete cover layer in compression) was approximately two times its negative flexural resistance (concrete top layer in tension). Bond between brick and concrete joints, which is the weakest link of this system, had marginal influence on the panel load carrying capacity. Shear failure was hard to obtain and seems to be of minor concern. Finally, a numerical model was developed to predict the deformational behavior of structural systems failing in bending. This model reproduced, with high accuracy, the load-deflection response registered in the tested panels.