Compatibility Torsion in Spandrel Beams Using Modified Compression Field Theory

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Compatibility Torsion in Spandrel Beams Using Modified Compression Field Theory

Author(s): Khaldoun N. Rahal and Michael P. Collins

Publication: Structural Journal

Volume: 103

Issue: 3

Appears on pages(s): 328-338

Keywords: beams; cracking; reinforced concrete; shear; spandrel beams; torsion

DOI: 10.14359/15310

Date: 5/1/2006

Abstract:
This paper describes a procedure that can be used to calculate the compatibility torsion in spandrel beams and other indeterminate structures. The procedure relies on the ability of the Modified Compression Field Theory (MCFT) to calculate cracked torsional and flexural stiffness for sections subjected to various combinations of stress resultants. The calculated ultimate loads are compared with the experimentally observed ultimate loads of 27 statically indeterminate floor beam-spandrel beam frames and very good agreement is observed. The comparison with the detailed experimental results shows that the MCFT is capable of accurately calculating the response of reinforced concrete sections subjected to combined shear, torsion, bending moment, and axial compression. The calculations of the proposed procedure also show that the strength of the frames is significantly larger than that calculated using the equations of the ACI and CSA codes due to the longitudinal restraint of the beams.