Title:
Graveyard Concrete
Author(s):
Billie G. Snell and Debby L. Amon
Publication:
Concrete International
Volume:
28
Issue:
3
Appears on pages(s):
66-67
Keywords:
cement plaster; cemetery; history; New Orleans
DOI:
Date:
3/1/2006
Abstract:
Designed in the tradition of European cemeteries, St. Louis No. 1 cemetery in New Orleans resembles a miniature French city. Most of the crypts and mausoleums in New Orleans are constructed of brick covered with a cement plaster, including one of the most famous crypts���that of the notorious Voodoo Queen, Marie Laveau.