207.1R-05: Guide to Mass Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 207.1R-05: Guide to Mass Concrete

Author(s): ACI Committee 207

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 30

Keywords: admixture; aggregate; air entrainment; batch; cement; compressive strength; cracking; creep; curing; durability; fly ash; formwork; grading; heat of hydration; mass concrete; mixing; mixture proportion; modulus of elasticity; placing; Poisson’s ratio.

DOI:

Date: 2/15/2006

Abstract:
Mass concrete is any volume of concrete with dimensions large enough to require that measures be taken to cope with the generation of heat from hydration of the cement and attendant volume change to minimize cracking. The design of mass concrete structures is generally based on durability, economy, and thermal action, with strength often being a secondary concern. This document contains a history of the development of mass concrete practice and discussion of materials and concrete mixture proportioning, properties, construction methods, and equipment. It covers traditionally placed and consolidated mass concrete and does not cover roller-compacted concrete.