A New, Simple, Practical Method to Characterize Toughness of Fiber-Reinforced Cement-Based Composites

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A New, Simple, Practical Method to Characterize Toughness of Fiber-Reinforced Cement-Based Composites

Author(s): Nabil H. El-Ashkar and Kimberly E. Kurtis

Publication: Materials Journal

Volume: 103

Issue: 1

Appears on pages(s): 33-44

Keywords: bending; fibers; flexure; toughness.

DOI: 10.14359/15125

Date: 1/1/2006

Abstract:
A simple and practical method to evaluate the toughness based on the flexural load-deflection curve is proposed, which overcomes many concerns surrounding the existing methods. The proposed method primarily considers the postcracking part of the loaddeflection curve. The advantages of characterizing toughness in this region are that composite behavior in that region is most affected by the type of reinforcement, and measurement errors are relatively small. By analyzing data from the literature, it was shown that this method can give similar results regardless of the method used for measuring deflection, making this method applicable to test facilities of varying sophistication. Some advantages of the proposed method include: clear identification of the first crack point, the use of toughness indexes that are independent of the first crack deflection (where measurement error is greater), and quantitative representation of the load-deflection curve shape through the use of four postcracking toughness indexes, or quantitative representation of the overall composite toughness through a single parameter.