Title: Tunnel Shotcrete Lining

Author(s): E. S. Plotkin

Publication: Concrete International

Volume: 3

Issue: 1

Appears on pages(s): 94-97

Keywords: mixers; mixing; mix proportioning; safety; shotcrete; specifications; tunnel linings

DOI:

Date: 1/1/1981

Abstract:
Eleven station construction contracts for the Washington Metro were completed utilizing many types of shotcreting equipment, materials, and methods with a resultant variety of problems. Shotcrete production recommendations are listed, compiled from personal experience and analysis of problems which developed on several Metro projects.