Routine Maintenance of Concrete Bridges

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Routine Maintenance of Concrete Bridges

Author(s): ACI Committee 345

Publication: Concrete International

Volume: 5

Issue: 10

Appears on pages(s): 13-24

Keywords: bridge decks; bridges (structures); cleaning; concrete pavements; control joints; drains; highway bridges; maintenance; slope protection; substructures; superstructures.

DOI:

Date: 10/1/1983

Abstract:
Various potential sources of distress and the possible areas affected in the roadway, superstructure, substructure, approaches, slopes, and channel of a bridge are described. Guidance for avoiding or correcting such troubles is also provided in the form of a day-to-day maintenance and preventive maintenance guide. The report is directed to the local maintenance supervisor who has responsibility for routine bridge maintenance.