Tests of Reinforced Concrete Beams with Corrosion-Damaged Stirrups

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tests of Reinforced Concrete Beams with Corrosion-Damaged Stirrups

Author(s): Christopher Higgins and William C. Farrow III

Publication: Structural Journal

Volume: 103

Issue: 1

Appears on pages(s): 133-141

Keywords: corrosion; damage; shear strength.

DOI: 10.14359/15094

Date: 1/1/2006

Abstract:
An experimental investigation of corrosion on the shear capacity of conventionally-reinforced concrete beams was conducted. Large-size specimens were constructed and the embedded stirrups were subjected to accelerated corrosion. Three different corrosion damage levels were produced. Specimens were inspected and rated per national guidelines prior to testing. The condition ratings, however, did not indicate significant distinction between specimens or indicate differentiation in capacity. Tests indicated that corrosion damaged specimens exhibited reduced shear capacity and reduced overall deformation at failure. Sequentially-damaged stirrups had significant impact on structural performance of the test specimens.


ALSO AVAILABLE IN:

Electronic Structural Journal