A Need for In Situ Testing of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Need for In Situ Testing of Concrete

Author(s): Robert E. Philleo

Publication: Concrete International

Volume: 1

Issue: 9

Appears on pages(s): 43-44

Keywords: concrete construction; cylinders; inspection; ready mixed concrete; strength; tests

DOI:

Date: 9/1/1979

Abstract:
There is a definite need for in situ testing to determine the compliance of structures with designs based on the ACI Building Code and to sort out responsibilities for various aspects of concrete handling during construction. This article covers the importance of concrete strength testing to insure construction safety, provide quality concrete, and provide documentation of properly placed concrete.