Use of Roller Compacted Concrete in Brazil

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of Roller Compacted Concrete in Brazil

Author(s): Francisco Rodrigues Andriolo, Gustavo Reis Lobo de Vasconcelor, and Humberto Rodrigues Gama

Publication: Concrete International

Volume: 6

Issue: 5

Appears on pages(s): 29-34

Keywords: compacting; concrete dams; costs; gravity dams; mix proportioning; placing; roller compacted concrete; tests; vibration

DOI:

Date: 5/1/1984

Abstract:
Roller compacted concrete (RCC) has been used in Brazil since 1976 and has been subjected to a number of studies. RCC allows continuous placement with the possibilites of time and cost economies in the construction of concrete gravity dams in that South American nation. This article also deals with laboratory studies, mix proportioning, placement procedures, and test methods.