Title: 334.3R-05: Construction of Concrete Shells Using Inflated Forms

Author(s): ACI-ASCE Committee 334

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 13

Keywords: dome; fabric; inflation; polyurethane foam; reinforcement; shotcrete; thin shell.

DOI:

Date: 9/16/2005

Abstract:

Note: 334.3R-05 is Out of Print. However, a PDF version is available.

This report provides information on the construction of structural concrete shells using an inflated form. Major facets of the construction process are covered, including foundations, inflation, monitoring, and backup systems. Other aspects, such as the geometric variations of inflated forms, thickness of polyurethane foam, and mixture proportions for shotcrete, are also considered.