207.4R-05: Cooling and Insulating Systems for Mass Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 207.4R-05: Cooling and Insulating Systems for Mass Concrete

Author(s): ACI Committee 207

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 15

Keywords: cement content; coarse aggregate; creep; formwork; heat of hydration; mass concrete; modulus of elasticity; precooling; postcooling; pozzolan; restraint; specific heat; strain; stress; temperature rise; tensile strength; thermal conductivity.

DOI:

Date: 8/15/2005

Abstract:
The need to control volume change induced primarily by temperature change in mass concrete often requires cooling and insulating systems. This report reviews precooling, postcooling, and insulating systems. A simplified method for computing the temperature of freshly mixed concrete cooled by various systems is also presented.