Concrete Finisher Certification

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Finisher Certification

Author(s): Beverly Garnant

Publication: Concrete International

Volume: 27

Issue: 12

Appears on pages(s): 18-21

Keywords: certification; finishing; flatwork

DOI:

Date: 12/1/2005

Abstract:
With the continual development of new concrete additives, types of concrete, and quality requirements, the finishing of concrete flatwork is becoming more and more complex, and the demand for highly skilled finishers is increasing. In this article, the process of obtaining ACI certification and how it can benefit you, your employees, or your project are explained.