Shear Strength of Deep Beams Subjected to Simultaneous Top and Bottom Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength of Deep Beams Subjected to Simultaneous Top and Bottom Loading

Author(s): S. C. Lee and W. B. Siao

Publication: Structural Journal

Volume: 91

Issue: 6

Appears on pages(s): 663-665

Keywords: deep beams; loads (forces); shear strength; web reinforcement; Structural Research

DOI: 10.14359/1493

Date: 11/1/1994

Abstract:
The effect of combined top and bottom loading simultaneously on reinforced concrete deep beams is investigated. Proposals are made for predicting shear strengths of such beams. Experimental results reported previously by other investigators are used for comparison and verification purposes with theoretical predictions. Good agreement between experiment and theory is observed; existing rules and recommendations are deemed too imposing.